Shop
Showing 81–96 of 411 results
PZT Lead Zirconate Titanate / PbZrxTi1-xO3
Purity99.9 - 99.99 %
Pb % Lead base
Standard AlloyPurityComposition
Pb - In99.9 - 99.99 %In % = 5 - 60 %
Pb - Sn99.9 - 99.995 %Sn % = 10 - 60 %
Pb - Sn - Ag99.9 - 99.99 %
PbS Lead Sulfide
Purity99.999 %
Density (g/cm³)7.50
Melting Point (°C)1114
Evaporation Temperature (°C)500
ShapeGranules
PbTiO3 Lead Titanate
Purity99.9 - 99.99 %
Density (g/cm³)7.52
PbWO4 Lead Tungstate
Dimensionsmax. Ø 2" × 100 mm
Growth TechniqueCzochralski
Orientation(101)
Dopingundoped
Surface1 side / 2 sides polished
StructureTetragonal
Lattice Constanta = 0.542 nm
c = 1.205 nmMelting Point1123 °C
Density8.28 g/cm3
Thermal Expansion Coefficient10.2 × 10-6 K-1
Refractive Index2.3 @ 500 nm
Hardness3.5 - 4 M
PbZrO3 Lead Zirconate
Purity99.9 - 99.99 %
Density (g/cm³)9.80
B4C Boron Carbide
Purity99.9 - 99.99 %
Density (g/cm³)2.52
Melting Point (°C)2763
B4C Boron Carbide
Purity99.9 - 99.999 %
Density (g/cm³)2.52
Melting Point (°C)2350
Evaporation Temperature (°C)2650
ShapeGranules
BN Boron Nitride
Purity99.9 - 99.99 %
Density (g/cm³)2.10
Melting Point (°C)2973
BN Boron Nitride
Purity99.9 - 99.999 %
Density (g/cm³)2.25
Melting Point (°C)3000
Evaporation Temperature (°C)1600
ShapeGranules
CdSe Cadmium Selenide
Dimensions10 mm × 10 mm × 0.5 mm
Growth TechniquePhysical Vapor Transport
Orientation(0001)
(11-20)
(10-10)Surface1 side / 2 sides polished
StructureHexagonal
Lattice Constanta = 0.429 nm
c = 0.702 nmMelting Point1268 °C
Density5.81 g/cm3
Thermal Expansion Coefficient6.26 × 10-6 K-1 @ a-Achse
4.28 × 10-6 K-1 @ c-AchseDielectric Constant10.2 @ 300 K
Thermal Conductivity0.04 W cm-1 K-1 @ 300 K
Electron Mobility900 cm2 V-1 s-1 @ 300 K
Band Gap1.74 eV
CdSe Cadmium Selenide
Purity99.9 - 99.999 %
Density (g/cm³)5.82
Melting Point (°C)1268