• CdSe Cadmium Selenide

    Add to list

    Dimensions10 mm × 10 mm × 0.5 mm

    Growth TechniquePhysical Vapor Transport

    Orientation(0001)
    (11-20)
    (10-10)

    Surface1 side / 2 sides polished

    StructureHexagonal

    Lattice Constanta = 0.429 nm
    c = 0.702 nm

    Melting Point1268 °C

    Density5.81 g/cm3

    Thermal Expansion Coefficient6.26 × 10-6 K-1 @ a-Achse
    4.28 × 10-6 K-1 @ c-Achse

    Dielectric Constant10.2 @ 300 K

    Thermal Conductivity0.04 W cm-1 K-1 @ 300 K

    Electron Mobility900 cm2 V-1 s-1 @ 300 K

    Band Gap1.74 eV