Shop

Showing 385–400 of 411 results

  • ZnSe Zinc Selenide

    Add to list

    Dimensions10 mm × 10 mm × 0.5 mm

    Growth TechniquePhysical Vapor Transport

    Orientation(100)
    (110)
    (111)

    Surface1 side / 2 sides polished

    StructureCubic

    Lattice Constanta = 0.567 nm

    Melting Point1517 °C

    Density5.264 g/cm3

    Thermal Expansion Coefficient7.1 × 10-6K-1

    Dielectric Constant9.7 @ 300 K

    Thermal Conductivity13 W cm-1K-1@ 300 K

    Electron Mobility500 cm2 V-1s-1@ 300 K

    Band Gap2.82 eV

  • ZnSe Zinc Selenide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)5.27

    Melting Point (°C)1525

  • ZnSe Zinc Selenide

    Add to list

    Purity99.999 %

    Density (g/cm³)5.2

    Melting Point (°C)1526

    Evaporation Temperature (°C)700

    ShapeGranules

  • ZnS Zinc Sulfide

    Add to list

    Dimensions10 mm × 10 mm × 0.5 mm

    Growth TechniqueBridgman

    Orientation(100)
    (110)
    (111)

    Surface1 side / 2 sides polished

    StructureCubic

    Lattice Constanta = 0.541 nm

    Melting Point1830 °C

    Density4.09 g/cm3

    Thermal Expansion Coefficient6.6 × 10-6K-1

    Dielectric Constant8.3 @ 300 K

    Thermal Conductivity16.7 W cm-1K-1@ 300 K

    Electron Mobility340 cm2 V-1s-1@ 300 K

    Band Gap3.54 eV

  • ZnS Zinc Sulfide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)4.09

    Melting Point (°C)1830

  • ZnS Zinc Sulfide

    Add to list

    Purity99.99 %

    Density (g/cm³)3.98

    Melting Point (°C)Sublimation

    Evaporation Temperature (°C)1100

    ShapeGranules

  • ZnTe Zinc Telluride

    Add to list

    Dimensions10 mm × 10 mm × 0.5 mm

    Growth TechniqueBridgman

    Orientation(100)
    (110)
    (111)

    Surface1 side / 2 sides polished

    StructureCubic

    Lattice Constanta = 0.610nm

    Melting Point1295 °C

    Density5.63 g/cm3

    Thermal Expansion Coefficient8.3 × 10-6K-1

    Dielectric Constant9.7 @ 300 K

    Thermal Conductivity0.108 W cm-1K-1@ 300 K

    Electron Mobility350 cm2 V-1s-1@ 300 K

    Band Gap2.23 eV

  • Sn Tin

    Add to list

    Purity99.9 - 99.999 %

    Density (g/cm³)7.75

    Melting Point (°C)232

  • Sn Tin

    Add to list

    Purity99.9 - 99.999 %

    Density (g/cm³)7.28

    Melting Point (°C)232

    Evaporation Temperature (°C)997

    ShapeGranules / Wire / Sheet

  • SnO2 Tin Oxide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)6.95

    Melting Point (°C)1630

  • SnO2 Tin Oxide

    Add to list

    Purity99.99 - 99.999 %

    Density (g/cm³)6.90

    Melting Point (°C)1127

    Evaporation Temperature (°C)600

    ShapeGranules

  • SnO2 / Pd Tin Oxide / Palladium

    Add to list

    Purity99.99 %

    CompositionPd % = 0.5 - 1 %

    ShapeGranules / Disks

  • SnO2 / Pt Tin Oxide / Platinum

    Add to list

    Purity99.99 %

    CompositionPt % = 0.5 - 1 %

    ShapeGranules / Disks

  • SnS Tin Sulfide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)5.22

    Melting Point (°C)882

  • Zr Zirconium

    Add to list

    Purity99.5 - 99.99 %

    Density (g/cm³)6.51

    Melting Point (°C)1855

  • Zr Zirconium

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)6.49

    Melting Point (°C)1852

    Evaporation Temperature (°C)1987

    ShapeGranules / Wire