LSCO Lanthanum Strontium Cobalt Oxide / LaxSr1-xCoO3
Purity99.9 - 99.99 %
LSMO Lanthanum Strontium Manganite / LaxSr1-xMnO3
Purity99.9 - 99.99 %
LSNO Lanthanum Strontium Nickelate / LaxSr1-xNiO3
Purity99.9 - 99.99 %
LaAlO3 Lanthanum Aluminate
Dimensions10 mm × 10 mm × 0.5 mm
max. Ø 3"Growth TechniqueCzochralski
Orientation(100)
(110)
(111)Dopingundoped
Surface1 side / 2 sides polished
StructureRhombohedral (Pseudo-Cubic)
Lattice Constanta = 0.382 nm
α = 90.5 °Melting Point2100 °C
Density6.52 g/cm3
Thermal Expansion Coefficient9.2 × 10-6 K-1
Dielectric Constant24.5
Hardness6.5 M
LaAlO3 Lanthanum Aluminate
Purity99.9 %
LaF3 Lanthanfluorid
Dimensions10 mm × 10 mm × 0.5 mm
max. Ø 50 mmGrowth TechniqueBridgman
Orientation(0001)
Dopingundoped
Surface1 side / 2 sides polished
StructureTrigonal
Lattice Constanta = b = 0.719 nm
c = 0.737 nm
α = β = 90 °
γ = 120 °Melting Point1493 °C
Density5.94 g/cm3
Thermal Expansion Coefficient11.9 × 10-6 K-1 @ a-Achse
15.8 × 10-6 K-1 @ c-AchseRefractive Index1.601 @ 0.7 μm
Hardness4.5 M
LaF3 Lanthanum Fluoride
Purity99.9 - 99.99 %
Density (g/cm³)6.00
Melting Point (°C)1490
LaF3 Lanthanum Fluoride
Purity99.9 - 99.99 %
Density (g/cm³)6.00
Melting Point (°C)1490
Evaporation Temperature (°C)1600 - 1800
ShapeGranules
LaNbO3 Lanthanum Niobate
Purity99.9 %
La2O3 Lanthanum Oxide
Purity99.9 - 99.99 %
Density (g/cm³)6.51
Melting Point (°C)2315
La2O3 Lanthanum Oxide
Purity99.9 - 99.99 %
Density (g/cm³)6.51
Melting Point (°C)2307
Evaporation Temperature (°C)1400
ShapeGranules / Disks
LaTiO3 Lanthanum Titanate
Purity99.9 - 99.99 %
Density (g/cm³)5.90
Melting Point (°C)1900
Evaporation Temperature (°C)2200
ShapeGranules
LiGaO2 Lithium Gallium Oxide
Dimensionsmax. Ø 30 mm × 50 mm
Growth TechniqueCzochralski
Orientation(100)
Dopingundoped
Surface1 side / 2 sides polished
StructureOrthorhombic
Lattice Constanta = 0.540 nm
b = 0.501 nm
c = 0.638 nmMelting Point1600 °C
Density4.18 g/cm3
Thermal Expansion Coefficient11.8 × 10-6 K-1 @ a axis
12.5 × 10-6 K-1 @ b axis
3.7 × 10-6 K-1 @ c axisDielectric Constant7.0 @ a axis
6.5 @ b axis
8.3 @ c axisHardness7.5 M
LiAlO2 Lithium Aluminate
Dimensions10 mm × 10 mm × 0.5 mm
max. Ø 2" × 10 mmGrowth TechniqueCzochralski
Orientation(100)
Dopingundoped
Surface1 side / 2 sides polished
StructureTetragonal
Lattice Constanta = 0.517 nm
c = 0.629 nmMelting Point1900 °C
Density2.62 g/cm3
Thermal Expansion Coefficient7.1 × 10-6 K-1 @ a axis
15 × 10-6 K-1 @ c axisHardness6.5 M
LiF Lithium Fluoride
Dimensionsmax. Ø 4” × 80 mm
Growth TechniqueBridgman
Orientation(100)
Dopingundoped
Surface1 side / 2 sides polished
StructureCubic
Lattice Constanta = 0.403 nm
Melting Point845 °C
Density2.60 g/cm3
Thermal Expansion Coefficient34.3 × 10-6 K-1
Refractive Index1.390 @ 11 μm
Hardness4 M
LiNbO3 Lithium Niobate
Dimensions10 mm × 10 mm × 0.5 mm
max. Ø 4"Growth TechniqueCzochralski
Orientation(1120) x-cut
(1010) y-cut
(0001) z-cutDopingundoped, MgO
Surface1 side / 2 sides polished
StructureTrigonal
Lattice Constanta = 0.515 nm
c = 1.386 nmMelting Point1250 °C
Density4.64 g/cm3
Thermal Expansion Coefficient15.4 × 10-6 K-1 @ a axis
7.5 × 10-6 K-1 @ c axisRefractive Indexn0 = 2.286 @ 632.8 nm
ne = 2.203 @ 632.8 nmHardness5 M