Shop

Showing 321–336 of 411 results

  • SrTiO3 Strontium Titanate

    Add to list

    Dimensions 5 mm × 5 mm × 0.5 mm
    10 mm × 10 mm × 0.5 mm
    max. Ø 30 mm

    Growth TechniqueVerneuil

    Orientation(100)
    (110)
    (111)

    Dopingundoped, Nb, Fe

    Surface1 side / 2 sides polished

    StructureCubic

    Lattice Constanta = 0.3905 nm (Perovskite)

    Melting Point2080 °C

    Density5.175 g/cm3

    Thermal Expansion Coefficient10.4 × 10-6 K-1

    Dielectric Constant300 @ 300 K

    Refractive Index2.25093 @ 2.48 µm

    Hardness6 M

  • SrTiO3 Strontium Titanate

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)5.11

    Melting Point (°C)2080

  • SrTiO3 Strontium Titanate

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)5.11

    Melting Point (°C)2080

    ShapeGranules

  • SrZrO3 Strontium Zirconate

    Add to list

    Purity99.9 - 99.99 %

  • Ta Tantalum

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)16.65

    Melting Point (°C)3017

  • Ta Tantalum

    Add to list

    Purity99.99 %

    Density (g/cm³)16.60

    Melting Point (°C)2996

    Evaporation Temperature (°C)2590

    ShapeGranules / Wire / Sheet

  • Ta2O5 Tantalum Oxide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)8.74

    Melting Point (°C)1800

  • Ta2O5 Tantalum Oxide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)8.70

    Melting Point (°C)1800

    Evaporation Temperature (°C)1950

    ShapeGranules / Disks

  • Te Tellurium

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)6.25

    Melting Point (°C)452

  • Te Tellurium

    Add to list

    Purity99.9 - 99.9999 %

    Density (g/cm³)6.25

    Melting Point (°C)452

    Evaporation Temperature (°C)277

    CompositionGranules

  • TeO2 Tellurium Dioxide

    Add to list

    Dimensions10 mm × 10 mm × 0.5 mm

    Growth TechniqueCzochralski

    Orientation(100)
    (110)
    (111)

    Dopingundoped

    Surface1 side / 2 sides polished

    StructureTetragonal

    Lattice Constanta = 0.481 nm
    c = 0.761 nm

    Melting Point730 °C

    Density5.99 g/cm3

    Thermal Expansion Coefficient19.5 × 10-6 K-1 @ a axis
    6.10 × 10-6 K-1 @ c axis

    Dielectric Constant25 @ a axis @ 100 KHz
    22 @ c axis @ 100 KHz

    Refractive Indexn0 = 2.260 @ 630 nm
    ne = 2.142 @ 630 nm

    Hardness4.5 M

  • Tb Terbium

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)8.22

    Melting Point (°C)1356

  • Tb Terbium

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)8.23

    Melting Point (°C)1356

    Evaporation Temperature (°C)1150

    ShapeGranules

  • Tb3Ga5O12 Terbium Gallium Garnet (TGG)

    Add to list

    Dimensionsmax. Ø 30 mm

    Growth TechniqueCzochralski

    Orientation(111)

    Dopingundoped

    Surface1 side / 2 sides polished

    StructureCubic

    Lattice Constanta = 1.236 nm

    Melting Point1725 °C

    Density7.13 g/cm3

    Thermal Expansion Coefficient9.4 × 10-6 K-1

    Refractive Index1.954 @ 1064 nm

    Hardness8 M

  • TbScO3 Terbium Scandium Oxide

    Add to list

    Dimensions10 mm × 10 mm × 0.5 mm

    Growth TechniqueCzochralski

    Orientation(110)

    Dopingundoped

    Surface1 side / 2 sides polished

    StructureOrthorhombic

    Lattice Constanta = 0.545 nm
    b = 0.575 nm
    c = 0.793 nm

    Melting Point2127 °C

    Density6.60 g/cm3

  • Tb4O7 Terbium Peroxide

    Add to list

    Purity99.9 - 99.99 %

    Density (g/cm³)7.30

    Melting Point (°C)Decomposition

    ShapeGranules / Disks